Extensive Q&A covering fiberglass, resins, gelcoat, PWC repair, tools, materials, safety, and maintenance. Use the search box to find specific topics or browse by section. Manufacturer links and technical references are listed at the end.

How to use this page

This FAQ is here to help you decide what needs immediate attention, what can wait, and what information to send when you ask for help. If you do not see your issue listed, send a few photos and a short description so we can point you to the right repair path.

  • Use the search box to jump to a topic fast.
  • Start with General and Maintenance for quick triage.
  • Check Resources at the end for manufacturer and safety references.

Quick checklist before you call

  • Take clear photos of the damage from a few angles.
  • Note whether the issue is cosmetic, structural, electrical, or related to the jet pump or engine.
  • Write down the year, make, and model if you have it.
  • Tell us whether the craft sits in saltwater, brackish water, or on a trailer.

General Questions

What services does Mobile Marine Doc provide?

Read answer
We provide mobile fiberglass/gelcoat repairs, PWC repair, emergency temporary patches, bonding, minor structural repairs, fairing and finishing, color matching, haul-out coordination for large jobs, and insurance documentation.

Which areas do you serve?

Read answer
Key West, Stock Island, Cudjoe Key, Boca Chica, Big Pine Key, and nearby Lower Keys locations. Remote jobs are quoted with travel time and logistics.

How much does a typical repair cost?

Read answer
Costs vary by scope. Small gelcoat touch-ups: $100–$400. Moderate laminate or patch repairs: $300–$2,000. Structural repairs and full refinishes: several thousand. A free inspection provides an accurate written estimate.

Technical Q&A: Resins, Gelcoat & Composites

What is the difference between polyester, vinylester, and epoxy resins?

Read answer
Polyester is economical and common for production boats; vinylester improves adhesion and blister resistance; epoxy gives superior strength and moisture resistance and is preferred for structural, laminated, or osmosis repairs.

What are the common fiberglass cloths and mats (woven roving, biaxial, chopped strand mat)?

Read answer
Chopped strand mat (CSM) conforms easily and is used for hand layups and cosmetic repairs. Woven roving and biaxial cloths have higher strength and are used where directional strength is needed. Unidirectional and stitched fabrics are used in performance laminates. Choose cloth based on structural requirements and finish needs.

What core materials are used (balsa, foam, honeycomb) and how are core repairs performed?

Read answer
Common cores include balsa, PVC foam, and honeycomb. Core repairs require removing damaged core to sound laminate, replacing or rebuilding the core with compatible material, and re-laminating with appropriate resin and cloth. For balsa, seal edges with epoxy to prevent future rot; foam cores use compatible adhesives and resin systems.

What adhesives and bonding agents are used for hardware and thru-hulls?

Read answer
Use marine-grade epoxy adhesives or polyurethane adhesives specified for above-water or underwater fittings. Fasteners should be bedded with appropriate sealants (polysulfide, polyurethane) and backed with proper backing plates. Follow manufacturer’s torque specs and use stainless or marine-grade fasteners.

Why are mix ratios and temperature control important when working with two-part resins?

Read answer
Correct mix ratio ensures full cure and expected mechanical properties. Temperature affects viscosity and cure speed; too hot or too much catalyst increases exotherm risking cracking or poor lamination. Use scale/precision measures and follow the technical data sheet.

What is vacuum bagging and when is it used?

Read answer
Vacuum bagging applies pressure uniformly to remove excess resin and air, producing stronger, lighter laminates and better fiber-to-resin ratio. Used for high-performance or structural laminates and composite fabrication in controlled environments.

What are common failure modes in fiberglass hulls?

Read answer
Impact damage, delamination from water ingress, core rot in cored laminates, gelcoat cracking from UV/age, and fatigue cracking around hardware. Regular inspection and early repair prevent larger failures.

Materials & Cloth

How do I choose fabric and resin for a repair?

Read answer
Match resin type to existing laminate (polyester to polyester where possible) unless upgrading (epoxy for structural). Choose cloth for strength requirements: CSM for cosmetic, woven/biaxial for structural. When in doubt, consult a tech sheet or the original builder’s laminate schedule.

Can composites be exposed to high heat and what causes distortion?

Read answer
Resins have glass transition temperatures (Tg). Exceeding Tg softens the laminate causing distortion. Use high-temperature epoxies or appropriate thermal barrier coatings where heat exposure is expected. Avoid excessive exotherm during cure on large thick laminates.

Processes, Tools & Best Practices

What surface preparation is required before bonding or laminating?

Read answer
Remove loose material, clean with solvent, sand to bright rough surface (profile), and remove dust with tack cloth. For epoxy over polyester, use an appropriate adhesion promoter or interlayer and test compatibility. Follow product TDS for recommended profile and cleanliness.

What PPE and ventilation are required for sanding and resin work?

Read answer
Use NIOSH-rated respirators for solvent or styrene vapors, P100 filters for dust, nitrile gloves for resins, eye protection, and hearing protection for power tools. Use respirators even for sanding cured composites and ensure adequate ventilation or use local extraction.

What tools are essential for mobile composite repairs?

Read answer
Basic toolkit: mixing cups and scales, spreaders, rollers, heat gun, orbital sander, various grit sandpaper, respirator, hand tools, vacuum pump (if vacuum bagging), portable generator, and finishing polishers. Keep spare consumables like peel-ply, release film, and mixing sticks.

Maintenance & Preventative Care

How do I protect gelcoat from UV and oxidation?

Read answer
Regular waxing with UV-protective wax, polish, or ceramic coating reduces oxidation. Keep boats out of direct sun where possible and address small gelcoat chalking before it becomes deeper degradation.

How should I prepare my boat for long storage?

Read answer
Drain systems, protect batteries, fog engines if required, clean hull and topsides, apply protectant, remove valuables, and store in a covered area. For long water storage, inspect through-hulls and zincs regularly.

PWC / Jet Ski Specific

What materials are common for PWC hulls and how does that affect repair?

Read answer
Many PWCs use rotomolded polyethylene which requires plastic welding or specialty adhesives; others are fiberglass or composite. Identify the material before selecting repair method.

Safety & Regulations

Where can I find Safety Data Sheets and technical data for products?

Read answer
Manufacturers provide SDS and TDS on their websites (links in External Resources). Always review SDS for PPE, first aid, and disposal instructions before using products.

External Resources & Manufacturer Links

Authoritative references, product data sheets, and safety documents:

If you have a specific list of original external links (Fiberglass Warehouse product pages, Awlgrip technical bulletins, etc.) paste them and they will be added as direct citations next to relevant answers.

Verified Marine Repair References

See our Marine Repair Resources & Citations for manufacturer and safety sources used in our recommendations.

Technical citations used in this FAQ

For resin compatibility and repair best practices, see WEST SYSTEM, Interlux/International, and Awlgrip. For material sourcing and product reference, see Jamestown and Fiberglass Warehouse. Full source list: Resources & Citations.

Verified technical claim notes

  • Two-part epoxy systems require the manufacturer’s exact resin-to-hardener ratio for intended cure and strength (WEST SYSTEM).
  • Surface preparation, contamination control, and coating compatibility are required for durable gelcoat/topcoat adhesion (Interlux/International; Awlgrip).
  • PPE and ventilation requirements must follow current chemical safety guidance and product SDS/TDS (OSHA).

Full source list: Marine Repair Resources & Citations.